View single post by David A Cherry
 Posted: Sat Dec 19th, 2020 07:37 pm
PMQuoteReplyFull Topic
David A Cherry



Joined: Sun May 12th, 2019
Location: Cincinnati, Ohio USA
Status: 
Offline
Rick Powell wrote: Louis they need to be put in a punch press to achieved the necessary force to form them, I have access to them but pretty sure if you check around the Redlands area you will locate one.You don’t need a punch press...A simple Hydraulic bottle jack will work, The brass will be very thin. You will need to allow for this.. If my memory serves me correctly I think it’s around 6% Stretch.. The brass will also need to be annealed....400° for an hour should do it...